Tianjin(TEDA) Iron & Steel Trade Co., Ltd
|
|
| |
|
|
|
|

|
|
|
Origin |
China |
Modified Coal Tar Pitch: Softening Point:105-110; QI:8-12; TI:26min; Ash content: 0.3max; Coking Value:55min.
Middle Temperature Coa Tar Pitch: Softening Point: 85-100; QI:10max; TI:15-25; Ash content :0.3max; Volatile matter content :58-68.
High Temperature Coal Tar Pitch: Softening Point : 120-124; QI:6-10; TI:26min; Ash content :0.3max; Sulpfur:0.6max.
|
|
|
|
| |
|
|
|